TY - GEN
T1 - Characterization of cellulose isolated from pinewood waste (Pinus merkusii)
AU - Azizah, Fathia Rahmatul
AU - Ikhtiarini, Nur
AU - Masruri, Masruri
AU - Srihardyastutie, Arie
AU - Rahman, Moh Farid
N1 - Publisher Copyright:
© 2022 Author(s).
PY - 2022/11/16
Y1 - 2022/11/16
N2 - Cellulose is one of the renewable natural resource materials that can be found in Indonesia. Cellulose can be synthesized from various parts of plants, such as pine trees. Pinewood waste is also known for its high amount of cellulose content. Thus, cellulose can be isolated from its pinewood waste. The necessary process in isolation is the removal of lignin and hemicellulose by extraction method using some solvents and heating. The bleaching method is carried out with hydrogen peroxide solution. This resulted in white bright cellulose with a yield of 58.40%. Cellulose result was obtained in the form of microcrystalline and further characterized by some instrumentation similar as x-ray diffractometer (XRD), scanning electron microscope (SEM), and Fourier-Transform infrared spectroscopy (FTIR). The crystallinity index of cellulose resulted from the isolation process is 55.20%, with morphological surface in the form of multisized agglomerated long fibers with an average particle size 125 μm. FTIR spectra showed some peaks at specific wavenumber indicating a typical function group of cellulose. Therefore, it can be concluded that pinewood waste can be used as a high-value cellulose material, with an easy and environmentally friendly method.
AB - Cellulose is one of the renewable natural resource materials that can be found in Indonesia. Cellulose can be synthesized from various parts of plants, such as pine trees. Pinewood waste is also known for its high amount of cellulose content. Thus, cellulose can be isolated from its pinewood waste. The necessary process in isolation is the removal of lignin and hemicellulose by extraction method using some solvents and heating. The bleaching method is carried out with hydrogen peroxide solution. This resulted in white bright cellulose with a yield of 58.40%. Cellulose result was obtained in the form of microcrystalline and further characterized by some instrumentation similar as x-ray diffractometer (XRD), scanning electron microscope (SEM), and Fourier-Transform infrared spectroscopy (FTIR). The crystallinity index of cellulose resulted from the isolation process is 55.20%, with morphological surface in the form of multisized agglomerated long fibers with an average particle size 125 μm. FTIR spectra showed some peaks at specific wavenumber indicating a typical function group of cellulose. Therefore, it can be concluded that pinewood waste can be used as a high-value cellulose material, with an easy and environmentally friendly method.
UR - https://www.scopus.com/pages/publications/85142891385
U2 - 10.1063/5.0100369
DO - 10.1063/5.0100369
M3 - Conference contribution
AN - SCOPUS:85142891385
T3 - AIP Conference Proceedings
BT - 3rd International Seminar on Smart Molecule of Natural Resources-Asian Federation Biotechnology, ISSMART-AFOB 2021
A2 - Fatchiyah, Fatchiyah
A2 - Sari, Dewi Ratih Tirto
A2 - Kurnianingsih, Nia
A2 - Safitri, Anna
PB - American Institute of Physics Inc.
T2 - 3rd International Seminar on Smart Molecule of Natural Resources-Asian Federation Biotechnology, ISSMART-AFOB 2021
Y2 - 25 August 2021 through 26 August 2021
ER -